Author:
Qu Guorui,Zhou Shiwei,Wang Huiyao,Li Bo,Wei Yonggang
Abstract
The production of ferronickel concentrate from low-grade nickel laterite ore containing 1.31% nickel (Ni) was studied by the non-melting reduction magnetic separation process. The sodium chloride was used as additive and coal as a reductant. The effects of roasting temperature, roasting duration, reductant dosage, additive dosage, and grinding time on the grade and recovery were investigated. The optimal reduction conditions are a roasting temperature of 1250 °C, roasting duration of 80 min, reductant dosage of 10%, additive dosage of 5%, and a grinding time of 12 min. The grades of nickel and iron are improved from 2.13% and 51.12% to 8.15% and 64.28%, and the recovery of nickel is improved from 75.40% to 97.76%. The research results show that the additive in favor of the phase changes from lizardite phase to forsterite phase. The additive promotes agglomeration and separation of nickel and iron.
Funder
National Natural Science Foundation of China
Subject
General Materials Science,Metals and Alloys
Cited by
9 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献