Fracture Strength of Thin Monolithic Zirconia Crowns with Varying Thickness and Configuration of Finish LinesAn In Vitro Study
Author:
Singh K.,Singh P.S.,Malhotra P.
Abstract
Aim- The current study sought to assess the fracture strength of thin monolithic zirconia crowns of varying thickness and finish line configuration. Study design- The current study was carried out to evaluate and compare the fracture strength of monolithic zirconia crowns with chamfers and radial shoulder finish lines of 0.5, 0.8, and 1.1 mm thickness. Result- Monolithic zirconia crowns with merely 0.5 mm reduction demonstrated adequate strength for use in posterior areas. On evaluation and comparison it was observed that no statistically significant difference was found in the fracture strength of monolithic zirconia crowns with different thicknesses and finish lines was investigated. Conclusion- The 0.5 mm thickness of monolithic zirconia crowns demonstrated significant fracture resistance to withstand physiological performance, regardless of finish line type.
Subject
General Medicine,Materials Chemistry,General Medicine,General Medicine,General Materials Science,General Medicine,General Medicine,Aerospace Engineering,General Medicine