Abstract

AbstractThe shear wall system is one of the most commonly used lateral load‐resisting systems in reinforced concrete (RC) high‐rise buildings. The present work is designed to investigate the behavior of reinforced shear walls upon their hybrid fiber ratio, the horizontal reinforcement ratio, and for the reinforcement aspect ratio. For this purpose, nine‐shear walls were manufactured. The same longitudinal reinforcement ratio and the steel and carbon fibers were the main design concept. Withal, the self‐compacting concrete with fiber hybridization was the general perspective for the RC. All the shear wall models were inspected not only for torsion, but also for the energy dissipation capacity, crack propagation, etc. Torsional moment capacity increased, when the hybrid fiber ratio rose up from 0% to 1.0% and then 1.5%. However, this increase was larger in case of increasing the hybrid fiber ratio from 0% to 1.0%. Increasing the hybrid fiber ratio from 1.0% to 1.5% did not result in a performance increase as in the first case. Increasing the fiber ratio from 0% to 1% and from 1% to 1.5% increased the maximum torsional moment between 7.39% and 33.41%. Torsional moment and twist angle capacities increase with the increase in hybrid fiber and horizontal reinforcement ratio and the decrease in the aspect ratio in RC shear walls. Withal, the energy absorption capacity, ductility, and stiffness are also increased as the hybrid fiber ratio. Increasing the hybrid fiber ratio decreased the crack density in the plastic hinge region. Decreasing the aspect ratio from 1.5 to 1.25 increased the dissipation energy capacity between 68.75% and 100%. The addition of 1.0% fiber, a significant increase in the value of ~30% and 53% was achieved stiffness after the crack.

Funder

Atatürk Üniversitesi

Publisher

Wiley

Subject

Mechanics of Materials,General Materials Science,Building and Construction,Civil and Structural Engineering

Cited by 2 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3