The present aims to evaluate the effect of adding Zn (0.5% and 9.0% in wt%) on phase transformation temperatures, microstructure coarsening, solidification parameters (cooling rate‐L and growth rate‐VL), macrosegregation, and mechanical properties of directionally solidified Sn‐34wt%Bi‐xZn alloys. The samples have been characterized by optical microscopy, scanning electron microscopy, X‐ray fluorescence, and X‐ray diffraction, in addition to Vickers microhardness and tensile tests. The CALPHAD method has been used for thermodynamic computations via Thermo‐calc software, in order to obtain thermodynamic data. The microstructure of Sn–Bi–Zn alloys is mainly dendritic, composed of a Sn‐rich matrix (β‐Sn) with Bi precipitates inside and surrounded by a Sn+Bi eutectic mixture of phases, predominantly observed at the coarse scale. Coarse Zn needles are also observed in the Sn‐34wt%Bi‐9wt%Zn alloy due to the high Zn content. On the whole, Zn provoked a coarsening of the dendritic arrangement. Moreover, Zn additions cause inverse segregation of Bi, as compared to the rather constant macrosegregation profile observed in the binary Sn–Bi alloy. On the whole, both additions of Zn (0.5 and 9.0) promoted increase in Vickers microhardness, yield strength (σY), and ultimate tensile strength (σu), however, causing an overall reduction in elongation‐to‐fracture (δ).
Funder
Fundação de Amparo à Pesquisa do Estado de São Paulo
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior
Reference51 articles.
1. Lead-free Solders in Microelectronics
2. A review of lead-free solders for electronics applications
3. Microstructure, Thermal and Wetting Properties of Sn-Bi-Zn Lead-Free Solder
4. T. European Parliament T. Council of the European Union Directive 2002/95/EC of the European Parliament and of the Council of 27 January 2003 on the restriction of the use of certain hazardous substances in electrical and electronic equipment 2003 p.209.
5. Microstructural discovery of Al addition on Sn–0.5Cu-based Pb-free solder design