Affiliation:
1. Institute of Technical Chemistry University of Stuttgart Pfaffenwaldring 55 70569 Stuttgart Germany
Abstract
AbstractHerein, desilication in increasingly harsh conditions was used to introduce mesopores into two different industrial ZSM‐5 catalysts (Si/Al ratio 11 or 29). For desilicated samples, increasing BET surface areas, mesopore volumes, and Si(OH) densities were noted. Brønsted acid site (BAS) densities increased upon desilication, as formerly inaccessible BAS in blocked pores became available, while the strength of the BAS was maintained upon desilication. Using KOH instead of NaOH as desilication agent can increase the mesopore volume generated per mass loss. The correlations between desilication strength and properties were largely determined by the parent Si/Al ratio. In general the introduced mesopores increased lifetimes in the ETA conversion, while additional Si(OH) groups introduced by desilication reduce the lifetime again. The lifetime is thus determined by a complex interplay of BAS density, improved reactant transport by introduced mesopores and Si(OH) density. There were no additional aromatics formed in desilicated samples during the conversion of ethanol and the samples were, in terms of aromatic yield, outperformed by a microporous parent. However, as result of longer lifetimes less ethanol was lost due to coke formation. It is concluded that desilication should be combined with other post‐modifications to increase aromatic production and lifetime.
Funder
Deutsche Forschungsgemeinschaft
Subject
Inorganic Chemistry,Organic Chemistry,Physical and Theoretical Chemistry,Catalysis
Cited by
5 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献