Affiliation:
1. Department of Mechanical Engineering University of Michigan Ann Arbor MI 48109 USA
2. Department of Materials Science & Engineering University of Michigan Ann Arbor MI 48109 USA
Abstract
AbstractAnode‐free manufacturing holds promise to enable high energy densities and lower Lithium (Li)‐metal solid‐state batteries (LMSSBs). Nevertheless, in contrast to thick Li foil (>50 µm), the stripping capacity of in situ‐formed Li (10–30 µm) is limited due to diminished creep flow, resulting in reduced accessible capacity. This study explores the correlation between stripping capacity and surface roughness of garnet Li7La3Zr2O12 (LLZO) solid electrolyte. The results reveal that stripping capacity can be enhanced through the surface modification of solid electrolytes. Additionally, this study scrutinizes the stripping behavior of in situ Li under intermittent‐current discharge conditions, which are more relevant to the operational conditions of electric vehicles (EVs). It is demonstrated that, when compared to constant‐current stripping, intermittent‐current stripping effectively suppresses void formation and enhances the stripping capacity of in situ Li by 40%. It is considered that the intermittent current inhibits the accumulation of Li vacancies, thereby delaying the void formation. These findings provide valuable insights into the development of high‐performance anode‐free LMSSBs for EVs.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献