Homogenization Study of Molybdenum and Copper in P/M Steel
-
Published:2022-03-15
Issue:
Volume:
Page:
-
ISSN:2307-1877
-
Container-title:Journal of Engineering Research
-
language:
-
Short-container-title:JER is an international, peer-reviewed journal that publishes full-length original research papers, reviews, case studies in all areas of Engineering
Author:
Rathore Sanjay S., ,Singh Mani Kanwar,Joshi Tilak C.,Dabhade Vikram V., , ,
Abstract
Homogenization of 3wt% Molybdenum addition in Fe-0.7C alloy in the presence of 2wt% Cu under sinter-forged condition has been carried out. Samples alloys have been fabricated by sinter-forging route using elemental powders. Sintering was carried out at 1150oC in N2-10%H2 atmosphere. The sintered samples were immediately forged using 100-ton friction screw forging press at the sintering temperature. Homogenization studies were carried out in two steps, the preliminary study was carried out on a press-sinter-forged compact while the final study was carried out on sinter-forged slab prepared by capsule forging. Homogenization temperature was kept at 1250oC (heating rate of 10oC / min) in flowing N2-10%H2 atmosphere for various durations between 1-5 hr. The extent of Mo and Cu dissolution in the Fe matrix of homogenized samples was ascertained using microstructural characterization under optical microscope, SEM and EDS analysis. The influence of initial powder particle size, sintering tempera ture and homogenization temperature & duration on homogenization behavior have been discussed in length.
Subject
General Engineering