Affiliation:
1. Department of Physical Metallurgy, TU Clausthal, Germany
Abstract
ARMCO-iron was cross-rolled in two different modes, i.e. with a rotation of the rolling direction
through 90° after each individual pass or after half of the reduction in thickness only. In the first case,
which corresponds to a truly tetragonal straight deformation path, the orientation {001}〈110〉
assumes an extremely high orientation density of 50 × random after 93% reduction. Besides this, the
texture contains a nearly ideal 〈111〉‖ND-orientation tube, the intensity of which increases to about
10 × random. The texture of the second mode is similar to that of the first one up to about 50%
reduction. After that the density in the orientation {001}〈110〉 decreases and increases again at the
highest deformation degrees. Two minor orientation components {001}〈100〉 and {011}〈100〉 were
found with intensities in the range of 3 to 5 × random at low deformation degrees of about 10%.