Affiliation:
1. Department of Prosthodontics, University Medical Center Goettingen, Robert-Koch-Str. 40, 37075 Goettingen, Germany
2. Private Practice, Geleitstr. 68, 63456 Hanau, Germany
Abstract
This study evaluated the marginal accuracy of CAD/CAM-fabricated crown copings from four different materials within the same processing route. Twenty stone replicas of a metallic master die (prepared upper premolar) were scanned and divided into two groups. Group 1 (n=10) was used for a pilot test to determine the design parameters for best marginal accuracy. Group 2 (n=10) was used to fabricate 10 specimens from the following materials with one identical CAD/CAM system (GAMMA 202, Wissner GmbH, Goettingen, Germany): A = commercially pure (cp) titanium, B = cobalt-chromium alloy, C = yttria-stabilized zirconia (YSZ), and D = leucite-reinforced glass-ceramics. Copings from group 2 were evaluated for the mean marginal gap size (MeanMG) and average maximum marginal gap size (AMaxMG) with a light microscope in the “as-machined” state. The effect of the material on the marginal accuracy was analyzed by multiple pairwise comparisons (Mann–Whitney, U-test, α=0.05, adjusted by Bonferroni-Holmes method). MeanMG values were as follows: A: 46.92 ± 23.12 μm, B: 48.37 ± 29.72 μm, C: 68.25 ± 28.54 μm, and D: 58.73 ± 21.15 μm. The differences in the MeanMG values proved to be significant for groups A/C (p=0.0024), A/D (p=0.008), and B/C (p=0.0332). AMaxMG values (A: 91.54 ± 23.39 μm, B: 96.86 ± 24.19 μm, C: 120.66 ± 32.75 μm, and D: 100.22 ± 10.83 μm) revealed no significant differences. The material had a significant impact on the marginal accuracy of CAD/CAM-fabricated copings.
Subject
General Immunology and Microbiology,General Biochemistry, Genetics and Molecular Biology,General Medicine
Cited by
26 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献