Reactions of Subcutaneous Connective Tissue to Mineral Trioxide Aggregate, Biodentine®, and a Newly Developed BioACTIVE Base/Liner

Author:

Karabulut Barış1ORCID,Dönmez Nazmiye2ORCID,Göret Ceren Canbey3ORCID,Ataş Cafer1ORCID,Kuzu Özlem1ORCID

Affiliation:

1. Health Sciences University Faculty of Dentistry Department of Pedodontics, Istanbul, Turkey

2. Bezmialem Vakif University Faculty of Dentistry Department of Restorative Dentistry, Istanbul, Turkey

3. Health Sciences University Department of Surgical Pathology, Bagcilar Research and Education Hospital, Istanbul, Turkey

Abstract

Aim. There is an increasing interest in the application of BioACTIVE materials to achieve hard tissue formation and maintain pulp vitality. Mineral trioxide aggregate (MTA) and Biodentine® are BioACTIVE materials used for pulp capping. Recently, dental researchers have produced BioACTIVE glass-incorporated light-curable pulp capping material. The study is aimed at evaluating the subcutaneous connective tissue reactions to MTA, Biodentine®, ACTIVA BioACTIVE Base/Liner. These materials were placed in polyethylene tubes and implanted into the dorsal connective tissue of Sprague Dawley rats. The presence of inflammation, predominant cell type, calcification, and thickness of fibrous connective tissue was recorded by histological examination 7, 30, and 60 days after the implantation procedure. Scores were defined as follows: 0 = none or few inflammatory cells, no reaction; 1 = <25 cells, mild reaction; 2 = 25 to 125 cells, moderate reaction; and 3 = ≥125 cells, severe reaction. Fibrous capsule thickness, necrosis, and formation of calcification were recorded. ANOVA and post hoc Dunnett’s tests were used for statistically analyses (p<0.05). Results. In terms of oedema, inflammation, fibrous capsule, and necrosis, no significant differences were found in any time period for any material. MTA and Biodentine® showed higher calcification than in the ACTIVA BioACTIVE on day 30, and the difference was statistically significant (p<0.05). After 60 days, while calcification was not seen in the control group, it was observed in the test groups. There was a statistically significant difference between the control and the others. Conclusion. All materials were well tolerated by the tissues in the 60-day evaluation period. One notable finding is the presence of dystrophic calcification in the connective tissue adjacent to the newly developed BioACTIVE Base/Liner material. Therefore, this new BioACTIVE Base/Liner material may be safely recommended to clinicians as a pulp capping material.

Funder

University of Health Sciences Hamidiye Scientific Research Projects Unit

Publisher

Hindawi Limited

Subject

Instrumentation,Atomic and Molecular Physics, and Optics

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3