Abstract
The kinetics and mechanism of the initial stages of electrocrystallization of nickel, iron and nickel-iron alloy were characterized for the process of electrolytic deposition from a solution based on deep eutectic solvent ethaline (liquid mixture containing choline chloride and ethylene glycol at a molar ratio of 1:2, respectively). The theoretical model developed by Scharifker and Hills was used to interpret the obtained experimental data. It was shown that the electrodeposition of nickel and iron obeys the patterns of three-dimensional instantaneous and progressive nucleation, respectively. It was concluded that the formation of iron nuclei occurs at a significantly lower rate than in the case of nickel. The kinetics of the initial stages of Ni–Fe alloy deposition obeys the mechanism of instantaneous nucleation. Thus, in the case of electrolytic deposition from ethaline-based solutions on a glassy carbon electrode, nickel imposes on iron not only its own region of electrode potentials where alloy deposition occurs, but also the type of mechanism of nucleation in the course of codeposition.
Publisher
SHEI Ukrainian State University of Chemical Technology
Subject
Materials Chemistry,General Chemical Engineering,Environmental Chemistry,General Chemistry
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献