Affiliation:
1. 1Research & Development Center, The Yokohama Rubber Co., Ltd. 2-1 Oiwake Hiratsuka Kanagawa, 254-8601 Japan; email: k-chino@mta.yrc.co.jp
Abstract
Abstract
Thermoreversible crosslinking rubber (TRC-IR) was easily synthesized by modification of isoprene rubber (IR) with maleic anhydride followed by the addition of 3-amino-1,2,4-triazole (ATA), in solid phase. The mechanical properties of the resulting rubber were more similar to the sulfur-vulcanized rubber than general thermoplastic elastomers (ex. SEBS). Although the tensile strength and elongation at break were lower than those of a corresponding sulfur-vulcanized rubber, the moduli were as high as those of sulfur-cured rubber. Re-molding of TRC-IR could be repeated more than 10 times without significantly changing its mechanical properties. Differential scanning calorimetry (DSC) and infrared analyses revealed that the superior mechanical properties and good recyclability are attributable to the strong hydrogen bonding. The TRC-IR showed an endothermic transition peak at around 185 °C on the DSC chart, indicating cleavage of the hydrogen bonding. Infrared analyses also revealed that the absorption peaks of carboxylic acid were shifted to a lower region by the strong hydrogen bonding. The thermoreversible crosslinking system was also applied to EPM, EBM (ethylene-butene rubber), and IIR. These rubbers also showed superior mechanical properties as well as excellent recyclability.
Subject
Materials Chemistry,Polymers and Plastics
Cited by
27 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献