1. 1Department of Polymer Technology, Royal Institute of Technology, 100 44 Stockholm, Sweden
Abstract
Abstract
From these results it is possible to draw the following conclusions: The primary protection against thermo-oxidative degradation comes from the butyl coating. The butyl coating works mainly by stopping diffusion of oxygen from the surrounding air, which is more important than stopping the antioxidant from diffusing out of the rubber, since the antioxidant effect is small.
Subject
Materials Chemistry,Polymers and Plastics