Author:
Salih A. A., ,Abad W. K.,Fadaam S. A.,Hussein B. H., , ,
Abstract
PbO NPs have been prepared by green synthesis. The diffraction patterns of α-PbO-NPs are shown by the XRD pattern, and the β-PbO-NPs have proven the tetragonal and orthorhombic structure. PbO has an optical energy gap of 4.2 eV. The FT-IR observed bond at 676 cm-1 attributed to the existence of PbO stretch. Nanoparticals with spherical and semi-spherical shapes are formed, as seen in the SEM image. The average particle size was under 100 nm. Fabrication and characterization of a high performance Ag/PbO/PSi/pSi/Ag heterojunction photodetector. The photodetector's responsivity was 0.7 A/W at 850 nm. The maximum detectivity and quantum efficiency spectra 1.009 ×1013 at 850 nm and 3×102 at 200nm which indicates that PbO NPs made using this technique have a good chance of being used to create porous silicon photodetectors with high performance heterojunctions.
Publisher
Virtual Company of Physics
Subject
Physical and Theoretical Chemistry,Condensed Matter Physics,General Materials Science,Biomedical Engineering,Atomic and Molecular Physics, and Optics,Structural Biology
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献