TiO2 metal oxide layers rich in Ti3AlC2 phase was successfully prepared on TC4 alloy by micro-arc oxidation (PECC or ASD) process. Analysis of the material phases contained in the PECC layer by X-ray diffractometry; scanning electron microscopy and energy spectroscopy were used to analyses the pores and elemental distribution on the surface of the specimens; the cross-sectional thickness of PECC layers were measured by metallographic microscope; confocal microscopy was used to measure the surface roughness of the sample; High temperature wear resistance of PECC layers with different Ti3AlC2 concentration was compared by tribological wear testing. The results show: 1) The incorporation of Ti3AlC2 particles plays an obvious catalytic role in the growth of PECC layer and the thickness is up to 74.74 μm; 2) When the concentration of Ti3AlC2 gradually increases, the PECC layers fluctuates obviously, and the deposition sealing effect is remarkable; 3) When the concentration is 4-6 g/L, the alloy has the best wear resistance, volume wear is only 1.98×10-4 mm3 /N·m. Experiments have shown that surface modification of the alloy using the PECC process can further broaden the application of the alloy in the field of anti-wear
Publisher
Virtual Company of Physics
Reference25 articles.
1. [1] F. H. Froes, H. B. Bomberger, JOM. 37(1985)28-37; https://doi.org/10.1007/BF03259693
2. [2] Q. J. Wang, J. R. Liu, R. Yang, JAM. 34(4) (2014)1-26; https://doi: 10.11868/j.issn.1005-5053.2014.4.001
3. [3] A. Pathania, S. A. Kumar, B. K. Nagesha, S. Barad, T.N. Suresh, Mate. Today: Proc. 45(2021)4886-4892; https://doi:10.1016/j.matpr.2021.01.354
4. [4] Y. Li, Z.L. Zhou, Y.Y. He, Materials. 17(1) (2024)65; https://doi.org/10.3390/ma17010065
5. [5] A. Festas, A. Ramos, J.P. Davim, Proc Inst Mech Eng B J Eng Manuf. 236(4) (2022)309-318; https://doi:10.1177/09544054211028531