Abstract
The present study revealed a low-cost process for utilizing desert sand for preparing nanosilica by sol-gel technique. This work required sodium hydroxide, concentrated hydrochloric acid, distillate water as raw materials, and Iraqi sand. Nanosilica sample was characterized by X-Ray Diffraction (XRD), scanning electron microscopy analysis (SEM), atomic force microscope(AFM), surface area (BET) method, and fourier transform infrared (FTIR). The XRD result of produced sample is referred to as amorphous silica, and it has a broad peak at 2Θ= 22° – 22.5 º. SEM showed spherical, agglomerated silica particles with a diameter range of 26.57–28.93 nm. In addition, the average particle size was 76.35nm, with a dimension range of 40-110 nm, and the surface area was 510.96 m²/g. The inclusion of hydrogen-bonded silanol groups (Si–O–H) at 3437.15 cm-¹ and siloxane groups (Si–O–Si) at 1087.85 cm-¹in the FTIR spectra.
Publisher
Petroleum Research and Development Center (PRDC)
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献