This paper was prepared for the SPE-European Spring Meeting 1972 of the Society of Petroleum Engineers of AIME, held in Amsterdam, The Netherlands, May 16–18, 1972. Permission to copy is restricted to an abstract of not more than 300 words. Illustrations may not be copied. The abstract should contain conspicuous acknowledgment of where and by whom the paper is presented. Publication elsewhere after publication in the JOURNAL OF PETROLEUM TECHNOLOGY or the SOCIETY OF publication in the JOURNAL OF PETROLEUM TECHNOLOGY or the SOCIETY OF PETROLEUM ENGINEERS JOURNAL is usually granted upon request to the Editor PETROLEUM ENGINEERS JOURNAL is usually granted upon request to the Editor of the appropriate journal provided agreement to give proper credit is made. Discussion of this paper is invited. Three copies of any discussion should be sent to the Society of Petroleum Engineers, P.O. Box 228, The Hague, The Netherlands. Such discussion may be presented at the above meeting and, with the paper, may be considered for publication in one of the two SPE magazines. SUMMARY OF PAPER This paper describes Shell's approach to the problem of possible corrosion in large diameter pipelines transporting possible corrosion in large diameter pipelines transporting sweet wet gas from offshore fields in the North Sea and elsewhere It is considered unrealistic to attempt to predict such corrosion as may occur by using the rough-and-ready criteria often found adequate, for example in the case of gas condensate wells. To obtain more suitable criteria, several series of laboratory tests have been carried out which have enabled the effect of the main variables to be evaluated. The laboratory results obtained have been compared where possible with cases of corrosion in the field. These tests and their interpretation are discussed. Broadly speaking, it is concluded that corrosion is likely to occur at an unacceptable rate in a wet major submarine pipeline at partial pressures of carbon dioxide lower than those which partial pressures of carbon dioxide lower than those which would be considered acceptable for other facilities. The practical consequence of this, is that the gas has to be dried practical consequence of this, is that the gas has to be dried offshore, and the operational and financial implications are described for the North Sea case. Some remarks are made on the possible use of inhibitors as an alternative to drying and reasons for the rejections of this course are explained. Introduction a) Sweet corrosion in ps-condensate wells, and in associated gathering systems, Ls a well-known phenomenon. While the mechanism of the attack is not fully understood, the factors which influence the rate of the corrosion can be evaluated in a roughly quantitative manner. Inspection methods for wells and gathering systems are available which in many cases enable a check to be made on corrosion intensity and location, and there are more or less effective remedial measures that can be applied. If a failure occurs, it may be serious but it is unlikely to be disastrous. It follows therefore that if some corrosion goes undetected, or if remedial measures prove less effective than hoped, there are not matters for major concern. b) The position with a major submarine pipeline is, however. quite different. The capital investment is very large, and serious corrosion would mean at best a very expensive repair, and at worst loss of the line. In either case there might be heavy contractual penalties for non-delivery of gas. For large submarine pipelines the rough-and-ready criteria (e.g. the often quoted 7 and 30 p.s.i. carbon dioxide partial pressures) sometimes used to predict corrosion in partial pressures) sometimes used to predict corrosion in gas condensate wells should not be applied. Effective inspection is impracticable and monitoring the rate of attack would be of doubtful validity. Furthermore remedial measures applicable to wells and gathering systems do not have sufficient reliability. For the joint Indefatigable to Bacton, 30" by 62.5 mile submarine line. Shell/Esso considered it necessary to obtain, by means of laboratory experiments, data which could be used with a greater degree of confidence than the criteria just mentioned, data which would facilitate taking the decision as to whether or not to go to the considerable expense of drying the gas offshore in order to eliminate the possibility corrosion. (Refer Appendices I and II). possibility corrosion. (Refer Appendices I and II).

Publisher

SPE

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3