Author:
Vicente Alvarez M.A.,Santisteban J.R.,Vizcaíno P.,Ribárik G.,Ungar T.
Funder
CONICET
IAEA
U.S. Department of Energy
Subject
Metals and Alloys,Polymers and Plastics,Ceramics and Composites,Electronic, Optical and Magnetic Materials
Reference44 articles.
1. The ductile-brittle transition of a Zirconium alloy due to Hydrogen;Huang;Scr. Metall. Mater.,1993
2. Brittle fracture induced by hydrides in zircaloy-4;Bai;Scr. Metall. Mater.,1991
3. In “Materials’ Ageing and Degradation in Light Water Reactors, Mechanisms and Management”, Ed. K.L. Murty, Woodhead Publishing Limited, 2013, page 52.
4. The influence of hydride size and matrix strength on fracture initiation at hydrides in zirconium alloys;Puls;Metall. Trans. A,1988
5. Delayed hydrogen embrittlement of Zr-2.5wt.%Nb;Simpson;J. Nucl. Mater.,1974
Cited by
57 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献