Author:
Neininger Susan M.,Staggs J.E.J.,Horrocks A.R.,Hill N.J.
Subject
Materials Chemistry,Polymers and Plastics,Mechanics of Materials,Condensed Matter Physics
Reference15 articles.
1. Complex char formation in flame-retarded fibre-intumescent combinations: physical and chemical nature of char;Kandola;Text Res. J.,1999
2. Complex char formation in flame-retarded fibre-intumescent combinations—IV. Mass loss and thermal barrier properties;Kandola;Fire Mater.,2000
3. Developments in flame retardants for heat and fire resistant textiles—the role of char formation and intumescence;Horrocks;Polym Degrad Stab,1996
4. Horrocks AR, Kandola BK, Myler P, Blair D. Burning behaviour of fiber-reinforced composites and the role of char formation. In: Polymeric materials: science and engineering, 2000. Washington, DC: American Chemical Society, 2000. p. 33–4.
5. Analysis of different kinetic models in the dynamic pyrolysis of cellulose;Conesa;Thermochim Acta,1995
Cited by
15 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献