1. T. Couvant, P. Moulart, L. Legras, P. Bordes, J. Capelle, Y. Rouillon, T. Balon, PWSCC of austenitic stainless steels of heaters of pressurizers, in: Proc. 13th Int. Conf. Environ. Degradation of Materials in Nuclear Power Systems–Water Reactors. CNS, CDROM, 2007.
2. NISA Report, Cracks on the Inner Surface of the Welds at Primary Water Inlet and Outlet Nozzle to Steam Generators (title translated), NISA, February 05, 2008.
3. T. Shoji, K. Sakaguchi, Z.P. Lu, S. Hirano, Y. Hasegawa, K. Fujimoto, Effect of cold work and stress on oxidation and SCC behavior of stainless steels in PWR primary water environments, in: Proc. Int. Symp. Fontevraud 7, SFEN, France, Paper No. A103T103, CDROM, 2010.
4. T. Shoji, G.F. Li, J.H. Kwon, S. Matsushima, Z.P. Lu, Quantification of yield strength effects on IGSCC of austenitic stainless steels in high temperature waters, in: Proc. 11th Int. Conf. Environ. Degradation of Materials in Nuclear Power Systems–Water Reactors, ANS, 2003, pp. 834–843.
5. Influence of Carbide Precipitation and Rolling Direction on Intergranular Stress Corrosion Cracking of Austenitic Stainless Steels in Hydrogenated High-Temperature Water