1. Ahmed, S.M., Maksimov, D., 1968. Studies of the double layer at the oxide–solution interface. Research Report R196, Mines Branch, Department of Energy, Mines and Resources, Ottawa, Canada, 104 p. (This was published as Ahmed, S.M., Maksimov, D., 1968. Studies of the oxide surfaces at the liquid-solid interface. Part II. Fe oxides. Can. J. Chem. 46, 3841–3846).
2. ASTM B330-88, 1988. Standard test method for average particle size of powders of refractory metals and their compounds by the Fisher Sub-Sieve Sizer, 3p.
3. Frothing behaviour of aqueous solutions of oleic acid;Atrafi;Miner. Eng.,2012
4. Ayres, D.E., 1963. A review of the mineralogy of some low grade South Australian iron ores in relation to beneficiation testing. Paper presented at the Annual Meeting of the AusIMM, 14–24 August, 1963.
5. Bollen, L., 1967. Preparation of iron oxide as pigment. Mining Review No. 121, Department of Mines, South Australia, pp. 37–39.