1. Metallographic investigation of the damage caused to GRP by the combined action of electrical, mechanical, and chemical environments;Harris;J Mater Sci,1984
2. Akhtar A, Nadeau JS, Wang JY, Romily DP, Taggart C. Brittle fracture of non-ceramic insulators. Report for the Canadian Electrical Association (186 T 350). Prepared by the British Columbia Hydro and Power Authority; September 1986.
3. Failure of high voltage electrical insulators with pultruded glass fiber-reinforced plastic cores;Owen;Composites,1986
4. Failure analysis of brittle fracture in nonceramic insulators;Akhtar;J Compos Technol Res,1987
5. Kumosa M, et al. Micro-fracture mechanisms in glass/polymer insulator materials under combined effects of electrical, mechanical and environmental stresses. Final Report to the Bonneville Power Administration, Electric Power Research Institute and the Western Area Power Administration, Oregon Graduate Institute, Portland, Oregon; July 1994.