Abstract
Zirconium diboride has been
cathodically electrodeposited from ZrO2
and B2O3 dissolved in an equimolar mixture of K2ZrF6+KBF4 at 600�. The
deposition process is controlled by the concentration of B2O3
in the molten salt solution, and at higher current densities zirconium is co- deposited.
Carbon dioxide is evolved simultaneously from a graphite anode.