This study reports the influence of the addition of Yttrium (wt.3%) on strain-rate sensitivity of Mg-6Sn alloy. The Mg-6Sn and Mg-6Sn-3Y alloys were made by using high pressure die-cast. The microstructural and X-ray diffraction results exhibited that the Sn3Y5 and MgSnY intermetallic phases were formed with addition of Y to the Mg-6Sn alloy. Furthermore, the grain structure of the Mg-6Sn alloy was changed from dendritic to globular with addition of Y. The strain-rate sensitivity value of the Mg-6Sn-3Y alloy is found higher than that of the Mg-6Sn alloy for all strain value. This result was attributed to the formation of new intermetallics (Sn3Y5 and MgSnY) and microstructure morphology (from dendritic structure to globular).
Publisher
Kütahya Dumlupinar Üniversitesi
Reference24 articles.
1. [1] Yang, H.P., Fu, M.W., To, S., Wang, G.C., (2016), Investigation on the maximum strain rate sensitivity (m) superplastic deformation of Mg-Li based alloy Mater. and Design 112, 151-159. http://dx.doi.org/10.1016/j.matdes.2016.09.066
2. [2] Nan, X.L., Wang, H.Y., Wu, Z.Q., Xue, E.S., Zang, L., Jiang, Q.C., (2013), Effect of c/a ratio on Schimd Factors in Hexagonal close-packed metals, Scrip. Mater. 68, 530-533. http://dx.doi.org/10.1016/j.scriptamat.2012.12.006
3. [3] Pekgüleryüz, K. U. Kainer, A.A. Kaya, first ed., Woodhead Publishing Limited, Philadelphia, (2013).
4. [4] Friedrich, B. Mordike, Springer, Verlag Berlin Heilderberg (2006).
5. [5] Sandlöbes, S., Zaefferer, S., Schestakow, I., S. Yi, Gonzalez-Martinez, R., (2011), On the role of non-basal deformation mechanisms for the ductility of Mg and Mg–Y alloys Acta Mater. 59, 429-439. Doi:10.1016/j.actamat.2010.08.031.