Layered MAX phase ternary compounds (M = early transition metals, A = group A elements, and X = C or N) show promise of wide applications in many applied fields because these compounds have combined ceramic and metallic properties. As an exemple of the MAX phase family, Ti3SiC2 exhibits a high melting temperature, high electrical and thermal conductivities, and an excellent resistance to oxidation and thermal shock. Particularly, it possesses unusual mechanical properties, such as easy machinability, high Young's modulus, thus it is considered as a candidate in advanced nuclear reactors.In this work, we investigate the effect of hydrogen and helium on the cleavage fracture of Ti3SiC2 in order to evaluate the reliability of Ti3SiC2 used in nuclear industry. We have performed first-principles mechanical calculations by using the density functional theory as implemented in the Cambridge Serial Total Energy Package code. Uniaxial tensile simulations along c-axis have been done to calculate the stress-strain curve and the cleavage energy for each interlayer of Ti3SiC2. It is found that Ti3SiC2 has the cleavage characteristics, and the habit cleavage plane starts from Si-Ti interlayer because of relatively weak Si-Ti bond. Hydrogen and helium always accumulate in the Si layer. Helium decreases largely the critical stress of cleavage fracture of Ti3SiC2. In contrast, hydrogen does not efficiently affect the cleavage fracture in Ti3SiC2. The difference between helium and hydrogen behaviors in Ti3SiC2 originates primarily from the difference of electronic hybridization with lattice atoms of Ti3SiC2. For helium, the neighboring Si atoms will be ejected by helium atoms, and the Si-Ti bonds will be broken, thus resulting in the cleavage fracture. However, for hydrogen, it is primarily hybridized with the s states of neighboring Si atoms, which does not severely disturb the p-d hybridization between Si and Ti atoms. Thus, the cleavage fracture from Si-Ti interlayer is hardly aggravated in the presence of hydrogen. Fortunately, Ti3SiC2 has a self-repair ability at high temperatures. It will desorb helium atoms at high helium pressure through Si layers. This behavior will alleviate the cleavage fracture induced by helium. In summary, Ti3SiC2 may be a potential material applied in light water or other fission reactors in the future.

Publisher

Acta Physica Sinica, Chinese Physical Society and Institute of Physics, Chinese Academy of Sciences

Subject

General Physics and Astronomy

Cited by 4 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3