Bismuth fluoroborate glasses with compositions xBi2O3·(40 − x)LiF·60 B2O3 (x = 0, 5, 10, 15, and 20) are synthesized by melt-quench method. XRD pattern is obtained for all the samples to confirm their amorphous nature. FTIR spectroscopy is carried out for the reported samples. It reflects the effect of replacement of a non-oxide group (LiF) with an oxide group (Bi2O3) in the glass network, due to the presence of the various absorption bands and their shifting with such replacement, assigning a role of network modifier to Bi2O3. Density and molar volume show an increase in their values with increase in Bi2O3 concentration. Theoretical optical basicity is calculated for the reported samples, which shows a decreasing trend with the increasing concentration of Bi2O3.
Funder
Council of Scientific and Industrial Research, India
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献