The high magnesium nickel laterite ore need first be dehydrated if it is
treated by the pirometallurgical means. The nickel laterite ore was
dehydrated in a laboratory scale sintering pot in this study. The dehydration
mechanism was studied by using the thermo-gravimetric (TG) tests,
differential thermal analysis (DTA), and X-ray diffraction (XRD) experiments.
The measurements indicated that chlorite (Fe,Mg,Al)6(Si,Al)4O10(OH)8 and
serpentine Mg21Si12O28(OH)34H2O are the primary phases, while FeO(OH) and
(Fe,Mg,)3Si4O10(OH)2 are the minor phases in the ore. The water in the ore
can be divided as free water, crystal water, and hydroxyl group. During the
heating process, the temperature range for the removal of the free water is
25~140?C, for the crystal water it is 200~480 ?C, and for the hydroxyl group
it is 500~800?C. The experiments with various coal dosages show that the
temperatures of off-gas and burden increase with an increase in coal dosage.
The sinter samples were analyzed using XRD. The results demonstrated that
olivine (Mg,Fe)2SiO4 and spinel MgFe2O4 are the main bonding phases.
Publisher
National Library of Serbia
Subject
Materials Chemistry,Metals and Alloys,Mechanics of Materials,Geotechnical Engineering and Engineering Geology
Cited by
17 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献