Experimental and numerical analyses of an U-bend tube made of an output inter-heater tube after exploitation

Author:

Pavkov Vladimir1,Bakic Gordana2,Maksimovic Vesna1,Petrovic Aleksandar2,Mitrovic Nenad2ORCID,Miskovic Zarko2

Affiliation:

1. University of Belgrade, Vinča Institute of Nuclear Sciences, Belgrade, Serbia

2. University of Belgrade, Faculty of Mechanical Engineering, Belgrade, Serbia

Abstract

One of the important tasks of evaluating the integrity of mechanical process elements and structures is to determine the local mechanical properties. In this paper, experimental and numerical analyses of the mechanical behavior of an output inter-heater tube, made of 12H1MF heat-resistant steel, was performed after 200,000 h of exploitation. During exploitation, the tube was exposed to various mechanisms of damage including gas corrosion. The tube was cut from a pipe system during reparations of a thermal power plant, and then cold-deformed by bending to obtain a U-bend tube, which was then used in the experiment. For this purpose, a specimen holder made of structural steel S235 was specifically designed to test such a sample. The U-bend tube was then exposed to the external compressive load during the experiment. Experimental research was based on the application of the 3D digital image correlation (DIC), while a finite element method (FEM) was applied in numerical simulation performed by using the Abaqus software package. The 3D DIC is an optical and contactless experimental method that allows measurements of displacement fields and deformations of geometrically complex structures. The Aramis system was used for the experimental analysis as well as for verification of the numerical model. During the experiment, the von Mises strain field was measured at the top of the U-bend tube, in the tightening zone, as it represents a critical place for crack initiation and propagation during the work of an inter-heater. Based on the obtained results and a comparative analysis of experimental and numerical values of the von Mises strain field at the U-bend tube, deviation of the model predictions of about 18 % was determined. The FEM predicted smaller values of the von Mises strain field compared to the DIC method. This is the result of an incomplete geometry applied in the model due to deformation that occurred in the bend zone of the U-bend tube, loss of material and the tube surface damage due to the influence of gas corrosion during 200,000 h of exploitation. Experimental analysis has confirmed that the U-bend tube, after 200,000 h of exploitation, can remain in service even if it is damaged due to the effect of gas corrosion.

Publisher

National Library of Serbia

Subject

General Chemical Engineering,General Chemistry

Cited by 2 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3