Affiliation:
1. Jilin University, Ministry of Education, College of Materials Science and Engineering, The key Lab of Automobile Materials, Changchun, China
Abstract
In this study, titanium boride (TiB) was used to make Al-TiB composites. The
contents of TiB added into Al matrix were 1 wt.%, 5 wt.% and 10 wt.%,
respectively. The composites were pressed at a pressure of 382 MPa and
sintered at 600?C for 4 hours. The microstructures and properties of
density, hardness and wear were investigated. Experimental results indicated
that, the composite with 5 wt.% TiB owned the highest relative density and
hardness among the three parameters. In addition, TiB particles dramatically
improved the wear resistance of the Al matrix and the more TiB content the
better of the wear resistance. That is, the composite with 10 wt.% TiB owned
the best wear resistance.
Publisher
National Library of Serbia
Subject
Materials Chemistry,Metals and Alloys,Condensed Matter Physics,Ceramics and Composites
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献