Affiliation:
1. CSIR- National Metallurgical Laboratory, Mineral Processing Division, Jamshedpur, India
Abstract
The present investigation deals with the sinterability of Goa (India) iron
ore having high Fe (65.2%) content. The sinter basicity (CaO/SiO2) and its
MgO were varied in the 2.0 to 2.5 and 1.5 to 3.0 range. The effect of process
variables on the quality parameters of sinter namely, tumbler index (TI),
reduction-degradation index (RDI) and reducibility index (RI) as well as the
productivity of sinter was studied. The studies have shown that the
consumption of coke (C: 74%) was inter-influenced by the sinter basicity and
its MgO content. Increasing the solid fuel consumption was not a viable
solution to improve TI and RI simultaneously. The content of coke in the mix
could be reduced to as low as 4% through `low temperature sintering? at the
balanced return fines recirculation (~ 33 wt. percent). The sintering indices
in terms of productivity of sinter and its quality improve quite
significantly at a higher sinter basicity (CaO/SiO2 ~ 2.5) and its lower MgO
content (1.5%).
Publisher
National Library of Serbia
Subject
Materials Chemistry,Metals and Alloys,Condensed Matter Physics,Ceramics and Composites
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献