Author:
Nascimento AR,Mantovani MB,Mendonça LCdO,Vesselovcz J,Pacheco RR,Pini NP,Sundfeld D
Abstract
SUMMARY
The two-step approach of applying hydrofluoric acid followed by silane is deemed the gold-standard surface treatment protocol before bonding to glass ceramics. Given hydrofluoric acid is a toxic conditioning agent and with the intention to simplify this step, the dental company Ivoclar Vivadent (Schaan, Lietchtenstein) released a self-etching ceramic primer, Monobond Etch & Prime in 2015, claiming that hydrofluoric acid and silane application would no longer be required prior to luting glass ceramics. Therefore, this clinical case report and retrospective analysis describes the replacement of unsatisfactory anterior veneers due to clinical failures for new feldspathic glass ceramic veneers, using the aforementioned self-etching ceramic primer. After two years, feldspathic glass ceramics presented satisfying clinical performance with absence of debonding, tooth sensitivity, recurrent carious lesions, or marginal infiltration.
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献