1. Increased surface coverage leads to less negative EA values at each surface, with a similar trend to that of the adsorption energies (Fig. 8b). The most negative EA values at 0.25 ML arise from the 4-coordinated sites (P) for all three differently terminated diamond surfaces, while the P+H (linear) site possesses the NEA at the 0.5 ML Sc-adsorbed bare and oxygenated diamond;The EA depends significantly on the location of the adsorbed Sc atoms, as for previously studied metal adsorbates