Abstract
Abstract
Heat treatable aluminium alloys of the 6xxx series are widely used in the hood, trunk and roof sections of a car body as they offer better corrosion resistance, high strength to weight ratio and excellent weldability characteristics. Gas metal arc welding (GMAW), a high productivity process is extensively employed in the automobile sector due to its ease of automation. HAZ softening is one of the most common problems that occurs during the welding of aluminium alloys by GMAW because of its high heat input. Cold metal transfer (CMT) is the most suitable welding process for welding aluminium alloys especially for controlling HAZ softening issues that occur due to the low heat input involved in this process. However, softening continues to exist in the welded joints. In this investigation, Post -weld heat treatment (PWHT) was employed to increase joint efficiency and to minimize the HAZ softening of AA6061-T6 aluminum alloy joints welded by GMAW and CMT. The results show that the tensile strength of a post-weld heat treated CMT joint is 10 % higher i. e., 242 MPa (76 % of joint efficiency), than that of the as welded CMT joint. This is due to the nucleation of strengthening precipitates in the weld metal and heat affected zone regions.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
17 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献