Microstructure, tensile strength and dry sliding wear studies of Al-15Si, Al-15Si-4.5Cu alloys with and without grain refinement and modifications are presented. Experimental alloys such as Al-15Si and Al-15Si-4.5Cu were conventionally melted and gravity die cast. For grain refinement, 1 wt.% of Al-1Ti-3B and for modification, 0.17 wt.% of aluminum phosphide (AlP) and 0.4 wt.% of Al-10Sr were added to the alloy melt. The results reveal refined microstructure due to grain refinement, modification, improved hardness, higher tensile strength and better sliding wear. Moreover, Al-15Si-4.5Cu alloy (untreated and treated) showed improved mechanical properties as compared to conventional hypereutectic Al–Si alloy.
Subject
Materials Chemistry,Metals and Alloys,Physical and Theoretical Chemistry,Condensed Matter Physics
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献