The aim of the investigation was to determine the effect of the different amounts of suberinic acid residues (SAR) (2%, 5%, 10%, 15%, 20%, 50%) introduced as a hardener to the adhesive mass-based on urea-formaldehyde (UF) resin on the mechanical and physical properties of manufactured solid birch wood bonded samples. The produced samples were compared to samples bonded with industrial UF resin without the addition of SAR. The scope of the work was to determine the shear strength, the share of in-wood damage, the contact angle, and the surface free energy (SFE) for wood and suberinic acid (SAR). The results show that increasing from 2-5% of SAR to 20% of SAR in the adhesive mass is not justified as there are no statistically significant differences between the mean values of shear strength for these four variants (2SAR, 5SAR, 10SAR, 20SAR).
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献