This work is devoted to anodic oxidation at low temperatures in the sulfuric acid electrolyte of the foundry aluminum alloy AK9ch, with a high silicon content. Optimal anodizing conditions were chosen for obtaining coatings with a hardness of more than 300 HV and a thickness of about 40 microns. With an increase in the thickness of the coatings by increasing the current density or anodizing time, their hardness begins to decrease. The resulting hard coatings are planned to be used on large parts obtained by casting aluminum alloy AK9ch.