Author:
Zheng-Cun Zhou,Xiao-Bin Zhu,Jie Du
Abstract
Abstract
The anelastic relaxation is measured at a low and high frequency from low to high temperature in some Ti alloys, most of which are usually recorded in the internal friction-temperature spectra. In this paper, the point-defect relaxation in β-Ti alloys is described and discussed. The point defects are the interstitial impurity atoms, substitution atoms and vacancies in β-Ti alloys. The reorientation of interstitial impurity O atoms around matrix Ti and substitute atoms produces Snoek-type peaks. The various interactions between the interstitial impurity atoms (O,N,et al.) and matrix atoms/substitute atoms (Ti, Nb,Mo,V,et al. ) can also produce a complex relaxation spectra consisting of several Snoek-type peaks. The concentrations of interstitial impurity atoms and the substitute atoms have important roles on the height and width of the Snoek-type peaks. The reorientation of defect pairs consisting of the interstitial impurity atoms and vacancies is also involved in the relaxation processes. At high temperatures, the Mo-Mo atom-pairs can be reoriented under the inducing of cycle stress and produce similar Zener relaxation peak.
Subject
Computer Science Applications,History,Education
Reference39 articles.
1. Characterization methods of carbon atom occupation and diffusion behavior in Steel;Zhang;Science Technology and Engineering,2022
2. Influence of substitutional atoms on the Snoek peak of carbon in b.c.c. iron;Saitoh;[J]. Acta Mater,2004
3. Snoek-type anelastic relaxation in sintered β-tpye Ti-Nb alloys;Zhou;Acta Physica Sinica,2019
4. Interdiffusion behavior of Ti-Mo binary system in β;Feng;phase.The Chinese Journal of Nonferrous Metals,2009
5. Application and research progress of body-centred-cubic;Xiang;Ti-Mo alloys. Journal of Mechanical Engineering,2017