Author:
Alias Suffi Irni,Johar Banjuraizah,Adam Syed Nuzul Fadzli,Taib Mustaffa Ali Azhar,Othman Fatin Fatini,Fhan Khor Shing
Abstract
Abstract
The porcelain formulation containing percentages of treated FGD sludge waste from 5% up to 15% in replacement of feldspar were prepared. The porcelain mixture formulation were mixed by high energy planatery mill at speed 300 rpm for 1 hours. The powder were compacted by using hydraulic press and sintered at temperature 1200 °C for 3 hours. The sintered samples were characterized using X-ray fluorescene (XRF), X-ray diffraction (XRD), Fourier Transform Infrared (FTIR) and Thermogravimetry/Differential scanning calorimetry (TGA/DCS). The primary effect concerning the addition of treated FGD sludge was the change of intensity composition (gypsum and anhydrate) in porcelain formulation. The XRD analysis has shown that the main component in sludge waste were gypsum and anhydrate.
Subject
General Physics and Astronomy
Cited by
1 articles.