Abstract
Abstract
Intermediate casing wear with a spiral scar is often found in ultra-deep wells in Tarim Oil Field. In this work, the mechanism of such wear, and the measures to reduce wear are analyzed. Comparing the geometric characteristics of the wear scars, the root cause is found that the effective inner diameter of the casing is smaller than the outer diameter of the drill pipe joint after the uncemented casing helically buckled. To analyze the main factors affecting the helical buckling of the casing, the classical pipe mechanics theory is used and Well-X in Tarim area is taken as an example. The results show that too small hanging weight is the main cause of helical buckling of the casing. Besides downhole high temperature and large hole diameter enlargement rate are also important factors. The main measures, such as increasing the hanging weight, installing centralizers, and using graded cementation, have been proposed to reduce wear.
Subject
General Physics and Astronomy
Reference10 articles.
1. Casing burst strength after casing wear;Wu,2005
2. A study of the buckling of rotary drilling strings;Lubinski,1950
3. Buckling of tubing in pumping wells, its effects and means for controlling it;Lubinski,1957
4. Helical buckling of tubing sealed in packers;Lubinski;Journal of Petroleum Technology,1962
5. Tubing and casing buckling in horizontal wells;Chen;Journal of Petroleum Technology,1990
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献