Author:
Golubev R M,Buslaev R D,Bakulin E M,Dzyubanenko S V
Abstract
Abstract
The paper presents the study of thermoelectric properties of bismuth tellurides obtained by the method of electrochemical deposition. Measurements of electrical conductivity and the Seebeck coefficient were carried out on a NETZCH SBA 458 Nemesis® measuring installation. Based on the obtained measurements, the following conclusions were made: for samples synthesized by the method of continuous electrochemical deposition, the maximum value of the Seebeck coefficient reached α = 14 μV / K, while for samples obtained by the pulse method α = 47 μV / K. It was also noted that after annealing, the samples showed an increase in the Seebeck coefficient up to 1.5 times. As a result of analyzing the measured thermoelectric characteristics, it was concluded that the method of pulsed electrochemical deposition is more efficient for obtaining high-quality thermoelectric materials.
Subject
General Physics and Astronomy
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献