Concrete as alkaline (pH ∼12,5) and moist material can cause deterioration of polyvinyl chloride (PVC) floor coverings and adhesives through alkaline hydrolysis. Attempts to prevent alkaline hydrolysis have mainly been made by installing PVC floor coverings above ‘dry-enough’ concrete or by using self-levelling low-alkali (pH ∼11…11,5) screeds between concrete and floor coverings. In this study, screed, adhesive and PVC floor covering combinations have been varied by using different floor covering conditions in laboratory test series. VOC emissions have been analysed from flooring material samples (Bulk-VOC). The test samples have been measured for two to three years after installing floor covering. According to the results, a 5 mm layer of low-alkali screed (pH less than 11,5) will effectively protect PVC flooring against alkaline hydrolysis. It could also be concluded that the pH level immediately under floor covering has a better correlation with VOC emission than the RH of concrete in the moment of installing the floor covering.
Subject
General Physics and Astronomy