Author:
Alt J.,Arutinov D.,Bezshyyko O.,Bretz T.,Brignoli A.,Conaboy A.,Deucher P.,De Paola F.,del Giudice G.,di Cristo C.,Fecarotta O.,Fiorillo A.,Fischer H.,Glückler H.,Grewing C.,Hollnagel A.,Lacker H.,Miano A.,Natour G.,Orlov V.,Prota A.,Rehbein F.,Reghunath A.,Salzano A.,Schaaf M.,Scharf C.,Schmidt J.,Schumann M.,Vagts A.,van Waasen S.,Wurm M.
Abstract
Abstract
We measured the surface tension of linear alkylbenzene (LAB)
HYBLENE 113 mixed with Diphenyloxazole (PPO) as well as of pure LAB
HYBLENE 113 as part of material studies for the liquid-scintillator
based surround background tagger (SBT) in the proposed SHiP
experiment. The measurement was performed using the iron wire method
and the surface tension for linear alkyl benzene HYBLENE 113 plus
PPO was found to be (30.0 ± 0.6) mN/m 22.0 ± 0.5°C and
for pure HYBLENE 113, (29.2 ± 0.6) mN/m at
21.0 ± 0.5°C.
Subject
Mathematical Physics,Instrumentation
Reference12 articles.
1. A facility to Search for Hidden Particles (SHiP) at the CERN SPS;Anelli,2015
2. The SHiP experiment at the proposed CERN SPS Beam Dump Facility;Ahdida,2021
3. Proof-of-principle measurements with a liquid-scintillator detector using wavelength-shifting optical modules;Ehlert;JINST,2019
4. The Wavelength-Shifting Optical Module;Bastian-Querner;Sensors,2022
5. JUNO Conceptual Design Report;Djurcic,2015