Affiliation:
1. Department of Materials Science, Kitami Institute of Technology, Kitami, Hokkaido 090-8507, Japan
Abstract
New soluble polyimides with inherent viscosities of 0.25–0.62 dl g−1 were synthesized from 3,6-diamino-9-alkylcarbazole and various aromatic tetracarboxylic dianhydrides by the conventional two-step method, including ring-opening polyaddition and subsequent thermally cyclodehydration. Most of the polyimides having hexyl alkyl chains were soluble in N-methylpyrrolidinone and m-cresol, while the polymers having ethyl chains were not soluble in organic solvents. The glass transition temperatures and 10% weight loss temperatures under argon of the polyimides having hexyl chains were in the ranges 232–269 °C and 485–518 °C, respectively.
Subject
Materials Chemistry,Organic Chemistry,Polymers and Plastics
Cited by
48 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献