Abstract
617B alloy is one of the alternative materials for ultra-supercritical power generating units, its microstructure will change during service under extremely harsh conditions. The research of precipitation behavior of 617B superalloy and other similar nickel-based superalloy during aging is summarized. It is concluded that the main phases of 617B superalloy during aging include γ’ phase, μ phase and M23C6 carbide. The precipitation behavior of the three phases is affected by aging temperature and aging time. The microstructure of materials has a direct influence on the properties of materials. Therefore, in the aging process of 617B superalloy, the creep property of the alloy will be affected by these phases. This paper summarizes the effect of these phases on the creep behavior of 617B superalloy. It is found that γ’ phase has a positive effect on the creep behavior of 617B superalloy, while μ phase has a negative effect. M23C6 has two-sided effects depending on its size.
Reference22 articles.
1. Research and Development of Heat Resistant Materials for Advanced USC Power Plants with Steam Temperatures of 700°C and Above;Fujio;Engineering,2015
2. Dissolution behavior of intragranular M23C6 carbide in 617B Ni-base superalloy during long-term aging;Xuemei;Journal of Alloys and Compounds,2019
3. The effect of heat treatments on the creep-rupture properties of a wrought Ni-Cr heat-resistent alloy at 973 K;Manabu;J Mater Sci,2010
4. Creep behavior of INCOLOY alloy 617;Cabibbo;J Mater Sci,2008
5. Microstructure evolution in Alloy 617 B after a long-term creep and thermal aging at 700°C;Magdalena;Materials Science & Engineering A,2018