Ge–Se–Te chalcogenide films with Ge content from 10% to 27% were prepared using thermal evaporation. The films were annealed with different times, and the changes of the linear refractive index and optical band gap of the films with different chemical compositions were investigated. It was found that, after 30 h of annealing, the Ge20Se8.5Te71.5 film exhibits the smallest change ratio in terms of linear refractive index (<0.5%), optical band gap (<1.5%), and thickness (<2.5%). Therefore, this component has the best optical stability in the Ge–Se–Te system studied in this paper. The optical band gap of Ge20Se8.5Te71.5 is about 0.8 eV, and the refractive index exceeds 3.4, which is beneficial to the applications in Te-based optical waveguide devices.
Funder
Natural Science Foundation of China
Zhejiang Provincial Natural Science Foundation of China
Natural Science Foundation of Ningbo
Subject
Metals and Alloys,Polymers and Plastics,Surfaces, Coatings and Films,Biomaterials,Electronic, Optical and Magnetic Materials
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献