Author:
Najar Kaleem Ahmad,Sheikh N.A.,Butt Mohammad Mursaleen,Shah M.A.
Abstract
Purpose
The purpose of this study is to investigate the mechanical and tribological properties of the synthetic diamond coatings deposited on WC-Co cutting tools for their prospective applications in mechanical industry. In this work, the concept of nanocrystalline diamond, microcrystalline diamond and multilayer-diamond coating systems were proposed and deposited on WC-Co substrates with the top-layer nanocrystallinity, optimum thickness and interfacial adhesion strength for load-bearing tribological and machining applications. Also, the overall mechanical and tribological properties of all synthetic diamond coatings were compared for the purpose of selecting a suitable type of protective layer used on the surfaces of WC-Co cutting tools or mechanical dies.
Design/methodology/approach
Smooth and adhesive single layered and multilayered synthetic deposited on chemically etched cemented tungsten carbide (WC-Co) substrates using predetermined process parameters in hot filament chemical vapor deposition (HFCVD) method. A comparison has been documented between diamond coatings having different nature and architecture for the purpose of studying their mechanical and tribological characteristics. The friction characteristics were studied experimentally using ball-on-disc type linear reciprocating micro-tribometer under the influence of varying load conditions and within dry sliding conditions. Nanoindentation tests were conducted on each diamond coating using Berkovich nanoindenter for the measurement of their hardness and elastic modulus values. Also, the wear characteristics of all sliding bodies were studied under varying load conditions using cumulative weight loss and density method.
Findings
Depositing any type of diamond coating on the cemented carbide tool insert increases its all mechanical and tribological characteristics. When using boron-doping onto the top-layer surface of diamond coatings decrease slightly their mechanical properties but increases the tribological characteristics. Present analysis reveals that friction coefficient of all diamond-coated WC-Co substrates decreases with the increase of normal load. Therefore, maintaining an appropriate level of normal load, sliding time, sliding distance, atmospheric conditions and type of diamond coating, the friction coefficient may be kept to some lower value to improve mechanical processes.
Originality/value
As the single layered synthetic diamond coatings have not given the full requirements of mechanical and tribological properties when deposited on cutting tools. Therefore, the multilayered diamond coatings were proposed and developed to enhance the interfacial integrity of the nanocrystalline and microcrystalline layers (by eliminating the sharp interface) as well as increasing the hardness of tungsten carbide substrate. However, when using boron doping onto the top-layer surface of diamond, coatings decreases slightly their mechanical characteristics but also decreases the value of friction coefficient.
Subject
Surfaces, Coatings and Films,General Energy,Mechanical Engineering
Reference20 articles.
1. Nano to micrometric HFCVD diamond adhesion strength to Si3N4;Vacuum,2007
2. Experimental investigation of the effect of system rigidity on wear and friction-induced vibrations;Journal of Lubrication Technology,1983
3. Interact ions among friction, wear, and system stiffness–part 1: effect of normal load and system stiffness;Scientific American,1984
4. The effect of sliding speed and normal load on friction and wear property of aluminum;International Journal of Mechanical & Mechatronics Engineering,2011
5. Adhesion and debonding of multilayer thin film structures;Engineering Fracture Mechanics,1998
Cited by
14 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献