1. [1] H. Takahashi, K. Tsutsumi, Structural distortion and reactivity of powder crystal, Ceramics 2 (1967) 99–108.
2. [2] M. Nikaido, S. Sano, F. Saito, Effects of grinding condition on synthesis of forsterite, J. Soc. Powder Technol., Japan 37 (2000) 176–182.
3. [3] T. Yokoyama, T. Kubota, G. Jimbo, The limit of grinding of alumina powder in water by a planetary ball mill, J. Soc. Powder Technol., Japan 29 (1992) 102–109.
4. [4] D. Lewis, M. W. Lindley, X-ray line broadening study of the introduction and removal of strain in some refractory oxides, J. Am. Ceram. Soc. 47 (1964) 652–653.
5. [5] Y. Kanno, Y. Kuwahara, S. Fujiwara, Properties of activated-Si3N4 powders, J. Cram. Association, Japan 92 (1984) 617–621.