Abstract
An in-depth study on the characteristics of coke in the hearths of blast furnaces is of great significance for explaining the mechanism of coke deterioration in blast furnaces. In the present work, the changes in macromorphology, degree of graphitization, and microstructure of the coke taken from different hearth locations of a 5,800 m3 superlarge blast furnace during its intermediate repair period were systematically studied. Significant differences were found between cokes obtained from the edge (“edge coke”) and from the center (“center coke”) of the hearth in terms of properties and degradation mechanisms. Edge coke was severely eroded by liquid metal, and only a small amount of slag was detected in the coke porosity, whereas center coke was basically free from erosion by liquid metal, and a large amount of slag was detected in the coke porosity. The degree of graphitization of edge coke was higher than that of center coke. The carburizing effect of liquid metal was the main cause of the degradation of edge coke and made it smaller or even disappear. Center coke was degraded due to the combination of two factors: slag inserted into micropores on the surface of center coke loosened the surface structure; and graphite-like flakes that appeared on the center coke surface lowered the strength and caused cracks in the surface.
Funder
Supported by National Key R&D Program of China
Publisher
Public Library of Science (PLoS)
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献