Wołczyński W.,Bydałek A.W.
Abstract
Abstract
The suspension of copper droplets in the slag is considered. The copper/slug suspension is delivered as the product from the direct-to-blister process which is applied in the KGHM – Polska Miedź (Polish Copper) S.A. factory. The droplets / slag suspension was treated by a special set of reagents (patented by the authors) to improve the coagulation process. On the other hand, the observations are made to estimate if the melting / reduction process in the furnace is sufficiently effective to avoid a remaining of carbon in the copper droplets. The coagulation process was carried out in the crucible (laboratory scale). However, conditions imposed to the coagulation / solidification process in the laboratory scale were to some extent similar to those applied usually in the industry when the suspension is subjected to the analogous treatment in the electric arc-furnace. Some suggestions are formulated how to improve the industrial direct-to-blister process.
Subject
Metals and Alloys,Industrial and Manufacturing Engineering
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献