Abstract
AbstractA combined process of carbothermal reduction in vacuum and acid leaching is proposed to produce TiC from titanium bearing blast furnace (BF) slag from Pan Steel in Panzhihua city in China. Thermodynamics calculation shows that TiC can be obtained in the appropriate temperature and pressure range. Moreover, the results of the experiment indicate that TiC can be prepared by the combined process. The optimized parameters include particle size of original slag ideally below 200 mesh, reduction temperature of 1400°C, pressure of 1~10 Pa and mass ratio of slag and reduction (carbon powder) of 100/38. The x value in TiC